Enter the project PIN code, then choose the actual atmospheric exposure. The estimate uses ISO 9223 first-year zinc corrosion-rate ranges; it is a screening tool, not a durability guarantee.

Indicative time to first maintenance—
ISO zinc corrosion range—

How to use it

Location helps.
Exposure decides.

A PIN code records project location, but a warehouse interior, sheltered structure and exposed coastal installation in the same area can have different corrosivity. Choose the exposure that matches the actual installation and project specification.

CategoryTypical descriptionZinc first-year corrosion rate
C1Very low≤ 0.1 µm/year
C2Low>0.1–0.7 µm/year
C3Medium>0.7–2.1 µm/year
C4High>2.1–4.2 µm/year
C5Very high>4.2–8.4 µm/year
CXExtreme>8.4–25 µm/year

Important: ISO 9223 rates are based on first-year exposure and should not be linearly extrapolated as a design guarantee. Long-term durability, local chloride/pollution, sheltering and project coating specification still need engineering review.